SAE AMS 5707 : 2017
SAE AMS 5707 : 2017
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS 57NI - 19.5CR - 13.5CO - 4.3MO - 3.0TI - 1.4AL - 0.05ZR - 0.006B CONSUMABLE ELECTRODE REMELTED OR VACUUM INDUCTION MELTED 1825 TO 1900 DEGREES F (996 TO 1038 DEGREES C) SOLUTION, STABILIZATION, AND PRECIPITATION HEAT TREATED