Table of Contents

1 Technical Approach/Report Organization and Scope
2 Acronyms and Abbreviations
3 Process Units
4 Damage Mechanisms
Bibliography

Abstract

Defines the materials, fabrication, and repair of austenitic stainless steels and Nickel-iron-chromium alloys in high temperature 565-760 degrees C (1050-1400 Degrees F) refinery services.